  • Model NumberRSW – 30KN
    Brand NameYM
    Payment TermsT/T, paypal
    Brief introduction:
    Testing machine is mainly used for non-metallic materials in conventional performance test of tensile, compression, bending at room temperature and in conventional performance test of the creep under high and low temperature, etc; If equipped with corresponding accessories, can also do other test methods of performance test, such as shear, peel, tear, etc. Product manufacturing and inspection standard GB/T16491 the electronic universal testing machine; GB / 2611 "tester general technical requirements"
    Technical indicators:
    1. The test force
    Biggest test force (kN) : 5, 10, 20 and 50 specifications
    Effective load range: 0.4% 100% FS (not step inside and outside)
    Bian: 1/240000
    Relative error value: plus or minus 0.5%
    2. The test speed
    Speed adjusting range: 0.001 to 500 mm/min (stepless speed regulation)
    Speed relative error: plus or minus 0.5%
    Well test force rate, uniform deformation rate control range: 0.01% ~ 5% FS/S
    Well test force rate, uniform deformation rate control error: plus or minus 0.5%
    Constant test force, constant deformation control range: 0.5% ~ 100% FS
    Constant test force, constant deformation control error: less than 10% for the value plus or minus 1% FS
    More than 10% for value plus or minus 0.1% FS
    3. The displacement (mobile beam)
    Measuring range: 0 ~ 999 mm
    Resolution: 0.001 mm
    Relative error value: plus or minus 0.5%
    4. Deformation (room temperature)
    Range: 50 mm (or) according to the needs of user
    Output (for) the range: 0-5 mm (or) according to the needs of user
    Effective range: 0.4% ~ 100% FS
    Resolution: 0.008 mm
    Relative error value: plus or minus 0.5%

     
     

     
  • Brief introduction:
    Testing machine is mainly used for non-metallic materials in conventional performance test of tensile, compression, bending at room temperature and in conventional performance test of the creep under high and low temperature, etc; If equipped with corresponding accessories, can also do other test methods of performance test, such as shear, peel, tear, etc. Product manufacturing and inspection standard GB/T16491 the electronic universal testing machine; GB / 2611 "tester general technical requirements"

     
Products
Analytical instruments
Physical property test
Environmental monitoring and analysis
Lab general equipment
About us
About this website
Our service
Product purchase
Contact Us

Newsletter

Make Sure you dont miss interesting happenings by joining our newsletter program.

Contact Us
+86-18620722006
instruments@instrumentstrade.com